Product Description: ● More advanced hydro-thermal process technology ● Impurities content: 0.01%, approx.1% of ordinary zirconia powder ● Sintering temperature: 1350 degrees, 11.76 %( energy saving 6.6%) ● Flexural strength: 1490 MPa, increased by24.17%. ● Uniform particle size of Nano-powders optimized the sintering properties ● Reducing chloride ion content: minimize the effect of chloride ion on ceramics
Composition ZrO2/Y2O3=97/3mol%
For more detailed powder characteristics, please email us at info@zirae.com